TY - JOUR
T1 - Low-Cycle Fatigue Life and Fatigue Crack Propagation of Sintered Ag Nanoparticles
AU - Shioda, Ryutaro
AU - Kariya, Yoshiharu
AU - Mizumura, Noritsuka
AU - Sasaki, Koji
N1 - Publisher Copyright:
© 2016, The Minerals, Metals & Materials Society.
PY - 2017/2/1
Y1 - 2017/2/1
N2 - The low-cycle fatigue life and fatigue crack propagation behavior of sintered silver nanoparticles were investigated using miniature specimens sintered at two different temperatures. The fatigue crack initiation life and fatigue crack propagation rate of sintered Ag nanoparticles were extremely sensitive to changes in the range of inelastic energy density and the cyclic J integral, exhibiting brittle characteristics, in contrast to tin-based lead-free solder alloys. With increasing sintering temperature, the fatigue crack propagation rate decreased. On the other hand, the effect of sintering temperature on the fatigue crack initiation life differed depending on the use of either a smooth specimen (low-cycle fatigue test) or notched specimen (fatigue crack propagation test). For the notched specimens, the probability of grain boundaries around the notch decreased due to increased sintering temperature. Therefore, the fatigue crack initiation life was increased with an increase in sintering temperature in the fatigue crack propagation test. In the smooth specimen, however, the fatigue life decreased with an increase in sintering temperature, as the elastic modulus of the specimen increased with increasing sintering temperature. In the low-cycle fatigue test, the specimen sintered with high internal stress started to develop crack initiation early, causing a decrease in the crack initiation life.
AB - The low-cycle fatigue life and fatigue crack propagation behavior of sintered silver nanoparticles were investigated using miniature specimens sintered at two different temperatures. The fatigue crack initiation life and fatigue crack propagation rate of sintered Ag nanoparticles were extremely sensitive to changes in the range of inelastic energy density and the cyclic J integral, exhibiting brittle characteristics, in contrast to tin-based lead-free solder alloys. With increasing sintering temperature, the fatigue crack propagation rate decreased. On the other hand, the effect of sintering temperature on the fatigue crack initiation life differed depending on the use of either a smooth specimen (low-cycle fatigue test) or notched specimen (fatigue crack propagation test). For the notched specimens, the probability of grain boundaries around the notch decreased due to increased sintering temperature. Therefore, the fatigue crack initiation life was increased with an increase in sintering temperature in the fatigue crack propagation test. In the smooth specimen, however, the fatigue life decreased with an increase in sintering temperature, as the elastic modulus of the specimen increased with increasing sintering temperature. In the low-cycle fatigue test, the specimen sintered with high internal stress started to develop crack initiation early, causing a decrease in the crack initiation life.
KW - Ag nanoparticles
KW - FEM
KW - fatigue crack propagation
KW - low-cycle fatigue
KW - sintering
KW - sintering temperature
UR - http://www.scopus.com/inward/record.url?scp=84994410022&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=84994410022&partnerID=8YFLogxK
U2 - 10.1007/s11664-016-5068-2
DO - 10.1007/s11664-016-5068-2
M3 - Article
AN - SCOPUS:84994410022
SN - 0361-5235
VL - 46
SP - 1155
EP - 1162
JO - Journal of Electronic Materials
JF - Journal of Electronic Materials
IS - 2
ER -