Pinning behavior in bulk MgB2 prepared using boron powder refined via high-energy ultra-sonication

Sai Srikanth Arvapalli, Muralidhar Miryala, Milos Jirsa, Naomichi Sakai, Masato Murakami

研究成果: Article査読

6 被引用数 (Scopus)

抄録

We successfully refined a cheap commercial boron powder by means of high-energy ultra-sonication and utilized it in synthesis of bulk MgB2. Rietveld phase analysis of X-ray diffraction pattern revealed completely formed MgB2 with a low amount of MgO. MgB2 bulk prepared of boron ultra-sonicated in ethanol for 15 min showed self-field Jc of around 300 kA/cm2 at 20 K without any compromise in Tc (~39 K). Pinning analysis based on Dew-Hughes expression showed major pinning contribution from grain-boundary pinning (~95.5%), along with a slight contribution from point pinning (4.5%). The microstructure study detected a system of large MgB2 grains (hundreds nm large) and 10–20 nm sized particles, possibly Mg-B-O, formed at MgB2 grain boundaries.

本文言語English
ページ(範囲)1297-1301
ページ数5
ジャーナルJournal of Superconductivity and Novel Magnetism
34
5
DOI
出版ステータスPublished - 2021 5月

ASJC Scopus subject areas

  • 電子材料、光学材料、および磁性材料
  • 凝縮系物理学

フィンガープリント

「Pinning behavior in bulk MgB2 prepared using boron powder refined via high-energy ultra-sonication」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル