N2 - It is reported that La-Al-Transition Metal alloys have high undercooled melt formation and high bulk amorphous formation ability by using rapid solidification process. We have examined the undercooling solidification and remarkable nucleation control behavior with adding SiC whisker by using containerless process. In this study, we investigated the undercooling, nucleation behavior and bulk amorphous formation for La 55Al 23Cu 10Ni 5Co 5 samples and samples with SiC whisker addition which are levitated and solidified by using the new gas jet flow and high cooling type electromagnetic levitation system. Therefore, the nucleation was controlled and the high undercooling degree, ΔT(= 0.22-0.28T m), was obtained with increasing SiC whisker addition. In addition, the bulk amorphous sample, φ7 mm sphere, was obtained at the cooling rate of levitating melt and solidification, about 100 K/s, for sample with 0.2% or more SiC whisker addition.
AB - It is reported that La-Al-Transition Metal alloys have high undercooled melt formation and high bulk amorphous formation ability by using rapid solidification process. We have examined the undercooling solidification and remarkable nucleation control behavior with adding SiC whisker by using containerless process. In this study, we investigated the undercooling, nucleation behavior and bulk amorphous formation for La 55Al 23Cu 10Ni 5Co 5 samples and samples with SiC whisker addition which are levitated and solidified by using the new gas jet flow and high cooling type electromagnetic levitation system. Therefore, the nucleation was controlled and the high undercooling degree, ΔT(= 0.22-0.28T m), was obtained with increasing SiC whisker addition. In addition, the bulk amorphous sample, φ7 mm sphere, was obtained at the cooling rate of levitating melt and solidification, about 100 K/s, for sample with 0.2% or more SiC whisker addition.
KW - Bulk amorphous
KW - Containerless process
KW - Gas jet flow type levitation apparatus
KW - High undercooling degree
KW - La Al Cu Ni Co alloy
UR - http://www.scopus.com/inward/record.url?scp=20844438161&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=20844438161&partnerID=8YFLogxK
U2 - 10.2320/jinstmet.69.399
DO - 10.2320/jinstmet.69.399
M3 - Article
AN - SCOPUS:20844438161
SN - 0021-4876
VL - 69
SP - 399
EP - 401
JO - Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals
JF - Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals
IS - 4
ER -